Diversity is only limited by imagination

PENOSIL PREMIUM GUNFOAM 65

Low-pressure, increased performance pistol foam for filling gaps
PENOSIL_Premium_Gunfoam_65_EN

logo2logo1

MATERIALS:
  • One-component increased performance polyurethane foam with homogeneous structure and low expansion, supplied in cans with aerosol
  • Light yellow color
  • Available in winter and summer versions
  • Adheres well to many building materials, except: Teflon, polyethylene and silicone surfaces
  • Provides very good sound and thermal insulation
  • Increased efficiency by 15% compared to standard can volume foam
  • Class F reaction to fire acc. PN-EN 13501-1+A1:2010.
INSTALLATION:
  • The surface on which the application is made must be free of dust, dirt and oil
  • The surface on which the application will be made should be well moistened. Lack of adequate humidity can cause secondary expansion
  • When applying in low temperatures, the can with winter foam version should be preheated in a warm place or water. Place or water temperature should not exceed + 30 ° C
  • Before use, shake the can with foam vigorously at least 20 times
  • The amount of foam discharged should be adjusted with use of the injection gun trigger.
  • After curing, the foam is not UV-resistant and must be covered within 24 hours. Unprotected foam gets brittle. The foam can be painted with water-based paints
  • Dirt from foam can be cleaned with Premium Foam Cleaner, Premium Foam Remover or with Premium Cleaning Wipes. Details are given in the cards of these products
  • Detailed information on storage, transport and safety are available in the safety data sheet (SDS).
Premium_Gunfoam_65_Letnia_1_140x360
Product code EAN code Kind Working temperature Volume Application Expiry date Version Package Outer cartoon
MIN MAX
- °C °C ml - months - pcs. pcs.
A1493 4742205009681 CAN WITH FOAM +5 +30 900 INJECTION GUN 18 SUMMER 1 12
A1540 4742640000793 CAN WITH FOAM -10 +30 900 INJECTION GUN 18 WINTER 1 12
Properties Unit Value
Tack free time minute 10-12
Cutting time (30 mm strap) minute 30-35
Completely cured in joint (in temperature +23 °C) hour up to 12
Completely cured in joint (in temperature +5 °C) hour up to 20
Density kg/m3 20-25
Fire class of cured foam (PN-EN 13501-1+A1:2010 ) - F
Volume decrease % non
Post-expansion % up to 33
Flash point of cured foam °C 400
Tensile strength (BS 5241 ) N/cm2 9
Compression strength at 10% deformation (DIN 53421 ) N/cm2 3
Thermal conductivity W/m*K 0,034
Sound reduction index dB RST,w = 60
Temperature resistance of cured foam °C long period: -50 to +90 short period: -65 to +130
The following values were obtained at temperature +23°C and 50% relative humidity, unless stated otherwise.